DATASHEET · SIDE BY SIDE
eSUN ABS+ vs Prusament ASA
From the Prusament ASA review: eSUN ABS+ is cheaper and tough, but degrades in sunlight; Prusament ASA is the pick whenever UV and weather resistance matter.
Measured wins
| Spec | eSUN ABS+ | Prusament ASA |
|---|---|---|
| Overview | ||
| Material | ABS | ASA |
| Manufacturer | eSUN | Prusa Polymers |
| Diameter | 1.75 mm | 1.75 mm |
| Thermal | ||
| Print temp | 220 to 260°C | 250 to 270°C |
| Bed temp | 80 to 110°C | 105 to 110°C |
| Warping | medium | medium |
| Quality | ||
| Layer adhesion | 5/5 | 5/5 |
| Bed adhesion | 4/5 | 4/5 |
| Stringing resistance | 3/5 | 3/5 |
| Verdict | ||
| Overall rating | 4.3/5 | 4.5/5 |
| Price / kg | — | — |
How they differ on the data
Prusament ASA runs 20°C hotter on the nozzle (window midpoints 240°C and 260°C), and the two windows share 10°C of range, so one profile can cover both. eSUN ABS+ lists the wider window (40°C against 20°C). Prusament ASA runs 13°C hotter on the bed (window midpoints 95°C and 108°C), and the two windows share 5°C of range, so one profile can cover both. eSUN ABS+ lists the wider window (30°C against 5°C).
Which one for the job
Pick eSUN ABS+ for enclosures.
Pick Prusament ASA for outdoor parts.