Polymaker PolyMide PA6-CF vs Taulman Bridge Nylon

From the Taulman Bridge Nylon review: PA6-CF is far stiffer and more dimensionally stable; Bridge is tougher under impact and much easier to print.

★ Best overall Polymaker PolyMide PA6-CF Polymaker · Nylon
Measured wins
Polymaker PolyMide PA6-CF: 2 Taulman Bridge Nylon: 1
Spec Polymaker PolyMide PA6-CFTaulman Bridge Nylon
Overview
Material Nylon Nylon
Manufacturer Polymaker Taulman3D
Diameter 1.75 mm 1.75 mm
Thermal
Print temp 280 to 300°C 250 to 260°C
Bed temp 25 to 50°C 70 to 110°C
Warping medium medium
Quality
Layer adhesion 4/5 5/5
Bed adhesion 3/5 3/5
Stringing resistance 4/5 3/5
Verdict
Overall rating 4.3/5 4.1/5
Price / kg — —

How they differ on the data

Polymaker PolyMide PA6-CF runs 35°C hotter on the nozzle (window midpoints 290°C and 255°C), and the windows do not overlap, so each needs its own profile. Polymaker PolyMide PA6-CF lists the wider window (20°C against 10°C). Taulman Bridge Nylon runs 52°C hotter on the bed (window midpoints 38°C and 90°C), and the windows do not overlap, so each needs its own profile. Taulman Bridge Nylon lists the wider window (40°C against 25°C).

Polymaker PolyMide PA6-CF ships on a 0.75 kg spool and Taulman Bridge Nylon on 0.45 kg, so compare price per kilogram rather than per spool.

Which one for the job

Pick Polymaker PolyMide PA6-CF for automotive.

Pick Taulman Bridge Nylon for living hinges.