DATASHEET · SIDE BY SIDE
eSUN eTPU-95A vs SUNLU TPU 95A
From the eSUN eTPU-95A review: The two budget 95A spools are close rivals. eSUN has the slightly better surface finish, SUNLU the slightly better price.
Measured wins
| Spec | eSUN eTPU-95A | SUNLU TPU 95A |
|---|---|---|
| Overview | ||
| Material | TPU | TPU |
| Manufacturer | eSUN | SUNLU |
| Diameter | 1.75 mm | 1.75 mm |
| Thermal | ||
| Print temp | 220 to 250°C | 210 to 230°C |
| Bed temp | 45 to 60°C | 50 to 60°C |
| Warping | none | low |
| Quality | ||
| Layer adhesion | 5/5 | 5/5 |
| Bed adhesion | 5/5 | 4/5 |
| Stringing resistance | 3/5 | 3/5 |
| Verdict | ||
| Overall rating | 4.2/5 | 4.3/5 |
| Price / kg | — | — |
How they differ on the data
eSUN eTPU-95A runs 15°C hotter on the nozzle (window midpoints 235°C and 220°C), and the two windows share 10°C of range, so one profile can cover both. eSUN eTPU-95A lists the wider window (30°C against 20°C). SUNLU TPU 95A runs 2°C hotter on the bed (window midpoints 53°C and 55°C), and the two windows share 10°C of range, so one profile can cover both. eSUN eTPU-95A lists the wider window (15°C against 10°C).
Which one for the job
Pick eSUN eTPU-95A for flexible parts.
Pick SUNLU TPU 95A for functional parts.